Z6CND17 11 is an austenitic stainless steel grade that offers a high corrosion resistance due to it’s broad composite of Molybdenum, particular effective against crevice and pitting corrosion. The austenitic structure of Z6CND17 also grants an excellent toughness, even at very low temperatures.
Base Element Fe (Iron)
Element | Min | Max |
---|---|---|
C (Carbon) | 0.07% | |
Cr (Chromium) | 16% | 18% |
Mn (Manganese) | 2% | |
Mo (Molybdenum) | 2% | 12% |
Ni (Nickel) | 10% | 12% |
P (Phosphorus) | 0.04% | |
S (Sulphur) | 0.03% | |
Si (Silicon) | 1% |
Mechanical Properties | Min | Max |
---|---|---|
Ultimate Tensile Strength (UTS) | 620 MPa |
Typically used within the Food and processing, petrochemical, subsea Industries for applications such as, boat fittings, heat exchangers, chemical transportation containers, bolting, springs etc.
Disclaimer:
Information is given for illustrative purposes only. Tachart accepts no responsibility for the accuracy of the data contained within or the use of the data by any other party.
This page is protected by copyright and may be freely distributed but not reproduced without permission.