Chemistry

Base Element Ni(Nickel)

Element Min Max
C (Carbon) 0.01%
Co(Cobalt) 2.5%
Cr(Chromium) 14.5% 16.5%
Fe (Iron) 4% 7%
Mn(Manganese) 1%
Mo(Molybdenum) 15% 17%
P(Phosphorus) 0.04
S (Sulphur) 0.03%
Si(Silicon) 0.08%
V(Vanadium) 0.35%
W (Tungsten) 3% 4.5%
Ni (Nickel) Balance
Mechanical Property Min Max
Ultimate Tensile Strength (UTS) 758 MPa
0.2% Proof Stress 363 MPa
Hardness (Rockwell B) 88 HRB
Elongation 62%

Heat Treatment; Normally solution heat-treated at 1121 degs C and rapid quenched.

Uses of Hastelly C276

Bolting
Bleach plants in the paper industry
Components exposed to sour gases
Sulphuric Acid reactors
Chloride processing Equipment
Evaporators, heat exchangers filters and mixers used in Sulphuric Acid Environments!

Disclaimer:
Information is given for illustrative purposes only. Tachart accepts no responsibility for the accuracy of the data contained within or the use of the data by any other party.
This page is protected by copyright but may be freely distributed but not reproduced without permission.

Hastealloy C276
error: Content is Copyright Tachart Bolt & Nut Manufacturing !!