A193 B7M
Alloy Steel
Element | Min | Max |
---|---|---|
C (Carbon) | 0.36% | 0.49% |
Cr (Chromium) | 0.75% | 1.2% |
Mn (Manganese) | 0.65% | 1.1% |
Mo (Molybdenum) | 0.15% | 0.25% |
P (Phosphorus) | 0.35% | |
S (Sulphur) | 0.04% | |
Si (Silicon) | 0.15% | 0.35% |
Mechanical Property | Min | Max |
---|---|---|
Ultimate Tensile Strength (UTS) | 690 MPa | |
0.2% Proof Stress | 550 MPa | |
Elongation | 18% | |
Gauge Length | A4D | |
Hardness (Brinell) | 235 HB | |
Hardness (Rockwell B) | 99 HRB |
Typical applications of A193 B7M include but are not limited too; fittings, flanges, valves, pressure vessels and other high pressure services.