708M40
42CD4
1.7225
42CrMo4
Element | Min | Max |
---|---|---|
C (Carbon) | 0.36% | 0.44% |
Cr (Chromium) | 0.9% | 1.2% |
Mn (Manganese) | 0.7% | 1% |
Mo (Molybdenum) | 0.15% | 0.25% |
Mechanical Property | Min | Max |
---|---|---|
Ultimate Tensile Strength (UTS) | 775 MPa | 925 MPa |
Yield Strength | 585 MPa | |
0.2% Proof Stress | 570 MPa | |
Elongation | 15% | |
Gauge Length | 5.65vSo | |
Hardness (Brinell) | 223 | 277 HB |
Charpy V-Notch Impact = Room Temp. | 50 Joules |
Disclaimer:
Information is given for illustrative purposes only. Tachart accepts no responsibility for the accuracy of the data contained within or the use of the data by any other party.