HASTELLOY C276
2.4819
NiM06Cr15
UNS N10276
Haynes TC16
ASTM F467
ASTM F468
ND16C15
AD NIC56D
Base Element Ni(Nickel)
Element | Min | Max |
---|---|---|
C (Carbon) | 0.01% | |
Co(Cobalt) | 2.5% | |
Cr(Chromium) | 14.5% | 16.5% |
Fe (Iron) | 4% | 7% |
Mn(Manganese) | 1% | |
Mo(Molybdenum) | 15% | 17% |
P(Phosphorus) | 0.04 | |
S (Sulphur) | 0.03% | |
Si(Silicon) | 0.08% | |
V(Vanadium) | 0.35% | |
W (Tungsten) | 3% | 4.5% |
Ni (Nickel) | Balance |
Mechanical Property | Min | Max |
---|---|---|
Ultimate Tensile Strength (UTS) | 758 MPa | |
0.2% Proof Stress | 363 MPa | |
Hardness (Rockwell B) | 88 HRB | |
Elongation | 62% |
Heat Treatment; Normally solution heat-treated at 1121 degs C and rapid quenched.
Uses of Hastelly C276
Bolting
Bleach plants in the paper industry
Components exposed to sour gases
Sulphuric Acid reactors
Chloride processing Equipment
Evaporators, heat exchangers filters and mixers used in Sulphuric Acid Environments!